hi,
weld factor z as regulated in EN 13480-3 clause 4.5 takes the value of:
1.0 for 100%NDT
0.85 for random NDT
0.7 when no NDT
what is the value of z when we have:
(100%ET + no random test) or ( no random + single butt)?
(in accordance with the EuroNorm)
regards,
 
thank you Andrei for your answer, I visited the outokumpu'site yesterday and I m really not sure,
z = 1.0 ?!!
regards
Leyla

 