Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Weld Heat Affected Zone (HAZ) 1

Status
Not open for further replies.

AWeld1

Computer
Joined
Jul 21, 2014
Messages
22
Location
QA
thread330-186625
Good Day!

I just would like to ask:
(1)is there any written code stating the removal of weld heat affected zone? If there is, can someone share this code for my reference?
(2) how do we remove have and up to what extent? how can we determine that size of weld HAZ?

Thank you
 
1) There is no Code mandating removal of the HAZ in carbon and low alloy steels.
2) For carbon and low alloy steels, the only effective way to remove the HAZ is to renormalize or anneal the weldment. Heat treatment must excced the upper critical temperature.
 
Thank you very much weldstan. Cheers.
 