baski67
Mechanical
- May 22, 2002
- 12
We are facing problem in weld repair of Super duplex grade 5A Casting to radiographic quality. Can anyone suggest tips on what care need to be taken especially in gauging and excavating the casting and also subsequent solution annealing of castings