lahane1443
Mechanical
- Oct 12, 2010
- 50
My welder has welded a test coupon of 1/2" OD with 5.0 mm thickness with GTAW process in 1G position,same welder has also welded a 6" OD coupon with 10.97 mm thickness in 1G position with GTAW process.He has passed RT test as required by ASME sec IX.
So can the same welder be used to weld a 48 mm OD pipe in 1G position for 15 mm thickness with GTAW process?
a quick reply is highly appreciated.
So can the same welder be used to weld a 48 mm OD pipe in 1G position for 15 mm thickness with GTAW process?
a quick reply is highly appreciated.