Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Welder Qualification for SA240 TP310S

Status
Not open for further replies.

balanayam777

Mechanical
Sep 5, 2014
1
Dear All,

I have a concern about welder qualification for SA240 TP310S .

Is it possible to qualify a welder in carbon steel and the same qualification covers for SA240 TP310S Material.

Since F no is same for Carbon steel and SS Materiel.


Please advice me.

Thanks in advance
 
Replies continue below

Recommended for you

balayanam,
"Is it possible to qualify a welder in carbon steel and the same qualification covers for SA240 TP310S Material."
What was the welding process and what was the filler metal of the original weld test ?
Regards,
DD
 
If the process is the same, the F number is the same, if the base metal used for the test is one listed by QW-423.1, and if the positions are appropriate as weld as the weld type (groove versus fillet weld): Yes

Best regards - Al
 
Does that mean you want to do so? Maybe. 310 is fully austenitic and prone to cracking. Some training in the proper techniques may be necessary.
 
The code lists the minimum requirements that must be met. It is up to the contractor to take what ever additional steps are necessary to ensure the product is safe.

Best regards - Al
 