Aloni
Mechanical
- Sep 7, 2013
- 36
Dear experts,
As far as I know when welding 304L to 304L the filler metal should be 308L.
My question is : can I weld 304L to 304L with filler metal 316-L ?
It’s a pressure vessel working in a full vacuum and + 0.7 barg at 250 ºc.
Material inside the vessel is not corrosive and suitable both 304L and 316L
regards
aloni
As far as I know when welding 304L to 304L the filler metal should be 308L.
My question is : can I weld 304L to 304L with filler metal 316-L ?
It’s a pressure vessel working in a full vacuum and + 0.7 barg at 250 ºc.
Material inside the vessel is not corrosive and suitable both 304L and 316L
regards
aloni