Jul 8, 2005 #1 TonyCro Mechanical Jan 12, 2005 23 0 0 GB Hello, I'm looking for a set of examples, hopefully with photos, showing general defects and causes. Any ideas? Many thanks TonyCro
Hello, I'm looking for a set of examples, hopefully with photos, showing general defects and causes. Any ideas? Many thanks TonyCro
Jul 8, 2005 #2 Carburize Materials Sep 23, 2002 702 0 0 US TWI in Cambridge England used to offer a set called "Faults in Fusion Welds in Constructional Steel" Upvote 0 Downvote
Jul 8, 2005 #3 metengr Materials Oct 2, 2003 15,478 0 0 US I saw this general web site from a previous post several weeks ago, and it contained some interesting links related to welding; http://www.khake.com/page89.html Upvote 0 Downvote
I saw this general web site from a previous post several weeks ago, and it contained some interesting links related to welding; http://www.khake.com/page89.html
Jul 8, 2005 #4 weldtek Materials Feb 12, 2005 897 0 0 US AWS has a publication called 'Welding Inspection Handbook' which is also an excellent reference. I think I paid around $75. for a copy. I recommend it highly. Upvote 0 Downvote
AWS has a publication called 'Welding Inspection Handbook' which is also an excellent reference. I think I paid around $75. for a copy. I recommend it highly.
Jul 8, 2005 #5 Rich2001 Mechanical Mar 23, 2001 896 0 0 US http://pntbeldyk.wirefire.com/ Vita sine litteris mors est. Upvote 0 Downvote
Jul 8, 2005 1 #6 pipewelder1999 Industrial Mar 17, 2002 305 0 0 US I have a few pictures here http://www.weldinginspectionsvcs.com/WorkPictures.htm . The Lack of Fusion, cracked tube to TS welds, and trapped slag pics may be useful. Have a nice day. Gerald Austin Iuka, Mississippi http://www.weldinginspectionsvcs.com Upvote 0 Downvote
I have a few pictures here http://www.weldinginspectionsvcs.com/WorkPictures.htm . The Lack of Fusion, cracked tube to TS welds, and trapped slag pics may be useful. Have a nice day. Gerald Austin Iuka, Mississippi http://www.weldinginspectionsvcs.com
Aug 24, 2005 #7 Emma1701 Automotive Aug 24, 2005 1 0 0 IT Talking about RSW, you can have a look at: http://www.romanmfg.com/files/imgTable.htm Bye. Emma Upvote 0 Downvote