Aug 31, 2007 #1 blckwtr Mechanical Oct 30, 2006 204 0 0 NO I have been searching the internet for formulas which cover my needs. I have found several pages, but the quality is poor. Does anyone know of a good site, or maybe litterature that has focus on stress calculations?
I have been searching the internet for formulas which cover my needs. I have found several pages, but the quality is poor. Does anyone know of a good site, or maybe litterature that has focus on stress calculations?
Aug 31, 2007 2 #2 metengr Materials Oct 2, 2003 15,478 0 0 US Yes. http://www.ecs.umass.edu/mie/labs/mda/dlib/machine/weld/weld.html OR purchase the following book Design of Weldments - Omer W. Blodgett Upvote 0 Downvote
Yes. http://www.ecs.umass.edu/mie/labs/mda/dlib/machine/weld/weld.html OR purchase the following book Design of Weldments - Omer W. Blodgett
Sep 1, 2007 #3 Lion06 Structural Nov 17, 2006 4,238 0 0 US Design of Welded Structures - also by Blodgett has good information on weld group properties. Upvote 0 Downvote
Sep 2, 2007 #4 msquared48 Structural Aug 7, 2007 14,745 0 0 US Blodgett is the structural engineer's bible on welding. If you do not have one - get it, read and use it. It's put out by Lincoln Arc Welding and has been around since the wheel was invented. Mike McCann McCann Engineering Upvote 0 Downvote
Blodgett is the structural engineer's bible on welding. If you do not have one - get it, read and use it. It's put out by Lincoln Arc Welding and has been around since the wheel was invented. Mike McCann McCann Engineering
Sep 11, 2007 1 #5 mwccwi Industrial Dec 26, 2006 6 0 0 US Here is another link that might help. Sorry so late http://www.engineersedge.com/weld_design_menu.shtml Upvote 0 Downvote
Here is another link that might help. Sorry so late http://www.engineersedge.com/weld_design_menu.shtml