Nov 21, 2018 #1 Menon5230 Mechanical Nov 21, 2018 5 0 0 OM Hai All, I want to weld a 1.5"weldolet to 8" pipe. The welder is qualified in 8" pipe full GTAW. This welder can weld this weldolet? Code is asme sec IX. This is a groove weld not fillet. Also thickness also need to consider? Menon
Hai All, I want to weld a 1.5"weldolet to 8" pipe. The welder is qualified in 8" pipe full GTAW. This welder can weld this weldolet? Code is asme sec IX. This is a groove weld not fillet. Also thickness also need to consider? Menon
Nov 22, 2018 #2 david339933 Industrial Jun 15, 2011 1,204 0 0 CA 8" Pipe performance will qualify 2-7/8" Min. Outside Diameter. - Table QW-452.3 Bonney Forge 1.5" Weldolet OD = 2-7/8" - Internet Bonney Forge 1.5" Weldolet Standard Weight Wall Thickness: 7/16" 8" Pipe Sch Std performance - .644" WM Qualified. Upvote 0 Downvote
8" Pipe performance will qualify 2-7/8" Min. Outside Diameter. - Table QW-452.3 Bonney Forge 1.5" Weldolet OD = 2-7/8" - Internet Bonney Forge 1.5" Weldolet Standard Weight Wall Thickness: 7/16" 8" Pipe Sch Std performance - .644" WM Qualified.