Welding of PQR coupons

Status
Not open for further replies.

cjgrass

Industrial
Apr 8, 2013
34
My question is does AWS D1.1 allow welding of PQR coupons to be outsourced, for example to a test facility, or does the welder have to be an employee of the contractor qualifying the procedures?
 
Replies continue below

Recommended for you

The latter is permitted. The former is not permitted.


Best regards - Al
 
Preparation and testing of mechanical specimens may be outsourced. Welding of the PQR coupon and associated certification of the PQR must be performed by the individual contractor or manufacturer.
 
Thanks a lot, that's what I thought but needed some back up.
 