Hi,
Has anyone got any good reference material in relation to how to assess if it is safe / or able to weld a collar onto a live water line? Am looking at welding a 20mm collar onto a 300NB water line, materials are: Collar = A516 Gr 60, pipe is A106 Gr B. Pressure in line is 6600KPag, with demin water flowing through it at
I'm interested in finding the basic process how this is assessed and the details involved. Are there any rule of thumb guidelines etc
Dave
Has anyone got any good reference material in relation to how to assess if it is safe / or able to weld a collar onto a live water line? Am looking at welding a 20mm collar onto a 300NB water line, materials are: Collar = A516 Gr 60, pipe is A106 Gr B. Pressure in line is 6600KPag, with demin water flowing through it at
I'm interested in finding the basic process how this is assessed and the details involved. Are there any rule of thumb guidelines etc
Dave