Will a PQR qualified using API 5L X42 (P1,G1) to A860 WPHY 42 (unassigned material) support a WPS for API 5L X52 to A860 WPHY 52? The API 5L X42 and API 5L X52 have the same P-number and Group-number. I am not familiar with the A860 WPHY fittings. Does the base metals qualified list in QW-424.1 apply to this application?