33
We are working with a sign company and need to weld sheets of alloy C22000 alloy to a bronze sculpture, C87300 alloy (Everdur). We are using tig but it doesn't seem to melt the metal very well at all. Any suggestions on a better way to weld this metal?

Thank you.
David
 
Replies continue below

Recommended for you

Oh, do not double post.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
C22000 is not a weldable alloy, due to zinc content. Brazing or soldering could work.
 
Braze. Don't try to weld these.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 