Can anyone help me I am looking for the Bearing Strength of Weldox 700 the datasheets only give tensile (ultimate and yield)

Thanks in advance
 
Replies continue below

Recommended for you

The bearing yield strength for most metals is approximately equal to the ultimate tensile strength. This type of information is not published widely, so you may need to test it yourself.