Jun 27, 2024 #1 mrmyagi Petroleum Feb 2, 2014 11 0 0 SE Hallo! What does g1 and g2 represent in EN13445-3 table A-7 figure F4 ? Could it have something to do with the throat thickness of the fillet welds? Thanks!
Hallo! What does g1 and g2 represent in EN13445-3 table A-7 figure F4 ? Could it have something to do with the throat thickness of the fillet welds? Thanks!
Jun 29, 2024 #2 r6155 Mechanical Jan 12, 2010 2,677 0 36 AR consider the side of the triangle. Regards Upvote 0 Downvote
Jun 29, 2024 Thread starter #3 mrmyagi Petroleum Feb 2, 2014 11 0 0 SE Ok, so g1 is the throat thickness * √2 ? Upvote 0 Downvote