Jul 8, 2015 #1 tarekdata Industrial Feb 12, 2007 20 0 0 SA Dear API std specialist. According to API 1104 , which pipe thickness tiger " threshold " starting Post welding heat treatment. Thanks Tarek
Dear API std specialist. According to API 1104 , which pipe thickness tiger " threshold " starting Post welding heat treatment. Thanks Tarek
Jul 8, 2015 #2 jte Mechanical Apr 8, 2002 2,357 0 0 US Hi Tarek- API 1104 is available at http://www.techstreet.com/api/products/1863960 Perhaps you will consider purchasing the standard which you seem to be using for your engineering or fabrication activities. That way, you will have it available as a ready reference. Upvote 0 Downvote
Hi Tarek- API 1104 is available at http://www.techstreet.com/api/products/1863960 Perhaps you will consider purchasing the standard which you seem to be using for your engineering or fabrication activities. That way, you will have it available as a ready reference.
Jul 9, 2015 #3 LittleInch Petroleum Mar 27, 2013 21,097 3 38 GB It's nothing to do with 1104 - it's to do with what the procedure requires which in turn, as a minimum, is what the design code requires. Remember - More details = better answers Also: If you get a response it's polite to respond to it. Upvote 0 Downvote
It's nothing to do with 1104 - it's to do with what the procedure requires which in turn, as a minimum, is what the design code requires. Remember - More details = better answers Also: If you get a response it's polite to respond to it.
Jul 20, 2015 #4 weldstan Materials Jun 24, 2011 2,730 0 36 US API 1104 does not provide the info regarding the thickness mandates for PWHT. B31.8 and B31.4 do. Upvote 0 Downvote
Aug 20, 2015 #5 Inspectoriam Petroleum Nov 8, 2013 5 0 0 US 1 1/4" is the thickness requireing PWHT within ASME B31.8 Gathering systems, this is the same as ASME B31.4 Upvote 0 Downvote
1 1/4" is the thickness requireing PWHT within ASME B31.8 Gathering systems, this is the same as ASME B31.4