I know there are lots of factors come into play when determine the bending stiffness. I am more concerned about the material and the design.
I'm using high carbon steel as the material. The density is 7490kg/m^3, Young Modulus=198000 MPa, and Poission's ratio=0.29.
I modeled the frames of the chassis using hollow rectangular tube. (One PHD student told me the hollow tube will give a better answer).
the value of bending stiffness is 31931.87866 N/mm
the value of torsional stiffness is 27646.14029 N.m/deg
please spare some times to answer
thanks
I'm using high carbon steel as the material. The density is 7490kg/m^3, Young Modulus=198000 MPa, and Poission's ratio=0.29.
I modeled the frames of the chassis using hollow rectangular tube. (One PHD student told me the hollow tube will give a better answer).
the value of bending stiffness is 31931.87866 N/mm
the value of torsional stiffness is 27646.14029 N.m/deg
please spare some times to answer
thanks