what is toughtriding? 1

Status
Not open for further replies.

sreedharkaipa

Materials
Jun 23, 2005
9
US
Hi,

Can any one tell me what is toughtriding? Any litrature references?

Any help is appreciated.

Thanks,
Sk
 
Replies continue below

Recommended for you

The term is "Tuftriding". It is cyanide based nitriding process used a lot for automotive crankshafts.