Apr 3, 2013 #1 petersi Automotive Feb 3, 2011 88 0 0 HK What is this grease? Aluminum grease? I see no where is selling grease at this silver color? thx
Apr 3, 2013 #2 M MintJulep Mechanical Jun 12, 2003 9,810 1 38 JP If I had to guess, oh wait I do have to guess, I'd guess that it's anti-seize. Upvote 0 Downvote
Apr 3, 2013 #3 CoryPad Materials Apr 15, 2002 5,192 0 0 US That is nickel-based anti-seize. Upvote 0 Downvote