Can anyone suggest a source for pre-made thin unidirectional/0 degree carbon fiber laminate sheeting with a thickness range of 0.1mm to 0.3mm?

 
Replies continue below

Recommended for you

There are a few guys, but try Coda composites in Winona MN, they can probably hook you up with small quantities of whatever you want for a price...
 
We have done many UD sheets in various thickness (0.2-3mm) for a costumer in the past. Tricky, but can be done as soon as you used a lot and effective release agent and be very careful when de moulding.
 