Hi,
I have stainless steel spiral railings where silica regularly brushes against(single piece vibrating bowl about 15 inches in diameter). These are most probably AISI 430. Though readily available, they wear up pretty fast. I need another material, but most tool steels cannot be made into railings economically. The replacement material should come in sheet form, can be formed into a spiral rail and still be wear and impact resistant. I'm at a loss as to what to select. Pls. help.
I have stainless steel spiral railings where silica regularly brushes against(single piece vibrating bowl about 15 inches in diameter). These are most probably AISI 430. Though readily available, they wear up pretty fast. I need another material, but most tool steels cannot be made into railings economically. The replacement material should come in sheet form, can be formed into a spiral rail and still be wear and impact resistant. I'm at a loss as to what to select. Pls. help.