Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

WPS by Section 4, with different thicknesses 1

Status
Not open for further replies.

Jeldon

Chemical
May 20, 2013
25
Qualification of WPS by Section 4, with different thicknesses 1/2'' x 2'', which will be the qualified range?
 
Replies continue below

Recommended for you

It is based on the thinner of the two members joined if you are working to D1.1.

Best regards - Al
 