WPS for tube welding

Status
Not open for further replies.

kkp3456

Petroleum
May 14, 2011
10
Usually the WPS made is considering the piping design. So is there any specific WPS for welding of tubes or do we apply the same rules for tubes as we do in for pipes?
 
Replies continue below

Recommended for you

A single WPS can be developed for both tubing and piping under ASME Section IX.
 
A single WPS can be developed to weld structural shapes, pipe, or tubing.

Best regards - Al
 