Which standard can be used as material specification & designation for wrapping tape? It's intend for buried pipeline.
 
Replies continue below

Recommended for you

EN 12068 will define the requirements for the tape coating. AWWA C209 may serve as an application specification. There are numerous other specifications that can be searched. Process Industry Practices may have something of use.