Aug 11, 2011 #1 fakhfakh Industrial Nov 11, 2004 48 0 0 TN I'm looking for the appropriate welding consumable for ZeCor-Z and ZeCor-310M plates welding having thickness 8mm. In addition is there any specific condition for preheating or PWHT? Welding process to be used: GTAW/FCAW or SAW Thank you
I'm looking for the appropriate welding consumable for ZeCor-Z and ZeCor-310M plates welding having thickness 8mm. In addition is there any specific condition for preheating or PWHT? Welding process to be used: GTAW/FCAW or SAW Thank you
Aug 11, 2011 1 #2 mrfailure Materials Aug 7, 2011 805 0 16 US Use ZeCor welding wire. Weldability is similar to 304/316 so I don't think you need preheat or PWHT. Upvote 0 Downvote
Aug 11, 2011 1 #3 EdStainless Materials May 20, 2004 15,892 0 0 US No preheat postheat, it is fully austenetic. too bad it isn't thinner, you could weld autogenous. You need matching alloy as filler. = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote
No preheat postheat, it is fully austenetic. too bad it isn't thinner, you could weld autogenous. You need matching alloy as filler. = = = = = = = = = = = = = = = = = = = = Plymouth Tube