Hello,

I have a zinc on zinc ball and socket joint that has a very low contact pressure in the joint but it stills wants to wear out. I am using Zamak 5 on Zamak 5.
Does anyone have any ideas on how to solve this wear problem?

I would like to remain with zinc die cast parts.

Thanks,

JJ
 
Replies continue below

Recommended for you

Lubricants: liquid (like oil) or solid films (like PTFE coating)

Hard coatings: diamond-like coating

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
I would suggest trying to make one of the parts harder. Either change alloys or use a coating. Only do one part. Then the soft one will wear, but the wear particles will cause minimal damage.

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
 