Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Aluminium Rectangular Hollow Section

Status
Not open for further replies.

JanekPop

Mechanical
Apr 23, 2003
16
I have been searching for a supplier of Aluminium Rectangular Hollow Section of size 40 x 25 x 2 mm with external corner radii of 2 or 3 mm. This external radius is important as a cosmetic/aesthetic feature in a design of a trolley. Sharper corners will not do. Most British suppliers only provide imperial sizes, but we want metric. Does anybody know where to find this size?

Thanks, Janek
 
Replies continue below

Recommended for you

This appears to be a size that could be easily extruded. Have you tried large producers like Alcoa, Hydro, Kaiser, etc.?
 
If this particular size of not available you can get an extrusion die made. Depends on your budget and quantities.
 