Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Requirements for Subsize Impact Specimens in PQR as per API 650

Status
Not open for further replies.

George VB

Mechanical
Aug 29, 2024
1
Dear Experts,

I am seeking clarification regarding the impact testing requirements for Procedure Qualification Records (PQR) as outlined in API 650, specifically Section 9.2.2.5.

We recently conducted impact testing using subsize specimens measuring 7.5 x 10 mm and obtained a value of 26J for P1 G2 material. However, the acceptance criteria according to API 650 9.2.2.5 is 27J.

Could you please confirm if there is any relaxation or allowance for subsize specimens in this context? If such allowances exist, could you provide guidance on where this information is detailed or any applicable references?

Thank you for your assistance.

 