Hello Expert,
Following are the situation,
Material, SA 312 Typ 304 L (Carbon content is >= 0.03 %)
Joining process :- Welding by GTAW process
Service Temprature -90 Degree (MAximum)
Pressure - 7kg/cm2 (maximum)
Service fluid :- Water,
Is IGC Test ( ASTM 262) is required to be carried out ...
Hello Expert,
I am seeking your technical advice in terms of Welding process.
For welding of crane girder we are using SMAW welding with root and hot pass DPT.
Now people want to change the welding process from SMAW to GMAW. (but root with SMAW)
Plate thickness ranging from 25 mm to 50 mm...
Hello Expert,
I am in a given situation that i am having a weld of SS 304L with SS 304L double V grove weld with root gap 3 mm and plate is made circular of dia 6000MM , thickness is 32 mm. The process is going to be used is GTAW for root and stabilizing pass and SMAW with fill-up and final...