Hello Expert,
Following are the situation,
Material, SA 312 Typ 304 L (Carbon content is >= 0.03 %)
Joining process :- Welding by GTAW process
Service Temprature -90 Degree (MAximum)
Pressure - 7kg/cm2 (maximum)
Service fluid :- Water,
Is IGC Test ( ASTM 262) is required to be carried out ?
As per my understanding, it is not required.
You please give your advice
Regards
HNJ
Following are the situation,
Material, SA 312 Typ 304 L (Carbon content is >= 0.03 %)
Joining process :- Welding by GTAW process
Service Temprature -90 Degree (MAximum)
Pressure - 7kg/cm2 (maximum)
Service fluid :- Water,
Is IGC Test ( ASTM 262) is required to be carried out ?
As per my understanding, it is not required.
You please give your advice
Regards
HNJ