Dear Colleagues,
I am aware all of above techniques. What I am asking, there is some time limit between P91 welding and PWHT, say 3, 7 or Max 29 days, if we do not organise PWHT within 29 days, it will lead us SCC crack. I am wondering to where I can get aforementioned info i.e time between...
Many thanks for your of your comments, as per my study,
According to Babcock & Wilcox, the time between completion of welding and PWHT should be limited to 14 days maximum to minimize the risk of SCC:
Gold M, Hainsworth J, Tanzosh J M, ‘Service experience with design and manufacturing...
I just want to some important/critical points on the subject:
The whole dispute we had on welding was the root pass for P91 for the first layer itself which should be 8 and above. However code allows after welding 1st layer PMI reading should be 7.2 and above.
ASME Section II part A calls...