  1. BoltSlinger

    Zinc per MIL-A-18001K

    A customer is wanting me to manufacture some Fasteners out of Zinc. I first thought they meant they wanted zinc plated Fasteners but after discussing it with their engineers the customer came back and confirmed the wanted Fasteners made from zinc. Not being familiar with zinc material (as bar...
  2. BoltSlinger

    API 20E Bolting

    Technically you can purchase from another vendor but it is a headache on the documentation end. We (Spring Bolt) are certified, but before we were most customers would not accept bolting that was not monogram. So we took the plunge, spend the money, and got our licenses (API Q1, 20E and now 20F)
  3. BoltSlinger

    Continuous cast steel making process is prohibited- API 20E

    Just to make I am following y'all: the ratio 10:1 could be the reason Continuous Cast is prohibited? CoryPad, Thank you!. I have spoken to Tata and it seems they will be able to help me. They have recommended a distributor here in Houston Metengr, Thank you, couple other requirements I...
  4. BoltSlinger

    Continuous cast steel making process is prohibited- API 20E

    API 20E BSL-3 states you can not use continuous cast steel. Looking at my historical 4140 MTRs all of it was made by means of continuous cast. I do not know my other options, or where to get material casted by other means. Any suggestions?
  5. BoltSlinger

    API 20E BSL-3

    Starting to dig into 20E. I do not believe I am picking up on everything required by me (the Manufacturer) under BSL-3. So things to look at when it comes to BSL-3: 1. Do not buy Continuous Cast steel, So buy "Ingot cast steel"? 2. chemical restrictions are met. 3. Re-Do Product analysis to...
  6. BoltSlinger

    API 6A Fasteners?

    Many companies are asking me to now quote ASTM A193, A194, A320, etc. to API 6A. I have tried reading through API 6A, and I am not seeing any modification to the ASTM specs. To me the the fastener specializations are called out in API 6A as a reference (when to use which bolt). Does that make...
  7. BoltSlinger

    IR-163 a lot of carbon

    anyone know any type of bar I can get with a carbon range of 70% to 82%? Thank you!
  8. BoltSlinger

    2,000 Degrees Fahrenheit

    What are some metals that are not effected by degrees up to 2,000 degrees fahrenheit?
  9. BoltSlinger

    B50A947A4 Material

    I thought that. I can only find one thing online that mentions the chem of it. I can not find a full GE write up specification.
  10. BoltSlinger

    B50A947A4 Material

    Anyone know anything about B50A947A4? I believe it is a 400 series stainless. I know B50A951A1 Stainless 422 Thanks ahead of time for any help on this.
  11. BoltSlinger

    "Ductility Test"

    Does anyone have any information on a ductility test. All I know is they mentioned 12%x4D. It sounds like they are talking about testing the elongation, but I am not sure. Thanks for the help!