Thank you MagBen!!
Is there this applicable in commercial scale or any industry person is using this method for UT testing as of now?
And please also provide some details on this. I have some papers and thesis but till now I didn't get enough idea how to perform on the sheets of dimension like...
Thanks a lot to all of you for your valuable support and prompt responses!!
Mr. MagBen, can you please provide some more insights on the doing the UT with 1.2 mm FBH and 2 mm FBH on 4 mm thickness!
Have any one tried this UT testing before? Please provide some reference publication (if any) for...
I am using 1.2 mm FBH for multiple discontinuity and 2 mm FBH (Flat Bottom Hole) for single/point discontinuity.
And I am trying with AMS 2632 standard.
Dear All!
Greeting from my side!!
I have gone through the Ultrasonic testing of the Alloy steel with Plate thickness > 6 mm. Now I am exploring to do the UT in final products [as thin sheets of Alloy Steel] in thickness 2-4 mm. First I have done with UT in 2-4 mm thickness with conventional...