Dear All,
which standard and level applicable for UT , for Forged Ring A105N OD 1580mm , ID 1275 mm and Th260 mm .
Please advise which standard is applicable to do such test (UT)?
From My side we Prepare this list , is it enough to grants the tubes will be manufactured with high quality
Chemical Analysis
1. Test Method for Chemical Analysis as Per ASTM E76.
2. Chemical Composition: shall conform to the composition limit specified in ASTM B165 Table.
3. Sampling: For...
Thanks Dear ,
My customer Requested from our side to do the following testing without mentioned standard :
- Chemical analysis.
- Mechanical, expansion and hardness
tests.
- Visual inspection & Dimensions check.
- Hydrostatic Test or its alternative
(nondestructive electric test) that...
Dear All ,
What is the the alternative of Hydrostatic Test to Tubes , is it Eddy Current Test ? am I right ? please advise ?
And should be tested as per ASTM E571 , By the way the tube should be manufactured as Per ASTM B165 ?
Thanks
Dear Stephen , Thanks
no, they are mentioned in Tender document the plate should be supplied ( Normalized and stress levied as per ASME BPVC II A2023, so for this requirement the plate should be normalized and stress relive should be applied it or no ?
?
Dear All ,
My Customer request from us to supply plate ( Normalized and stress relived ) , but the mill offer only normalized , we can consider the proposed specification by the mill comply with customer specification or we need to ask the mill for stress relived process to be applied , please...