I'm doing a little research on this project I'm working on. One application involves brazing a 316SS ring onto 13Cr pipe. Problem is, this thing will possibly see some high H2S environments (its going downhole). Now I've heard that even with a higher nickel content of braze, that the brazed...
griffengm, the application is room temperature. Its a room temperature cure, sets up in around 8 minutes and hardens to a rubber like consistency. But I'll still look in Carr just to see.
In order to check thread profiles on our parts, we use a product called ReproRubber. Its a two part mixture that when mixed and placed over the threads, it hardens and allows us to verify the profile. This stuff is rather expensive and we are looking for alternative solutions.
I've found a...
Trumpetman,
There are a few companies out there. One that was recommended to me was Solid Technologies. There was another topic that was discussing some of these with contact information. http://www.eng-tips.com/gviewthread.cfm/lev2/16/lev3/58/pid/380/qid/6250