Mike,
I wish there was room in these tanks for some of the ideas you guys mentioned.
http://www.myfilestash.com/userfiles/STENCH999/BLACK%20OXIDE1.JPG
http://www.myfilestash.com/userfiles/STENCH999/BLACK%20OXIDE2.JPG
the only room i can use inside these POS tanks is pretty much just below...
After talking to a local distributor, he suggested a Little Giant model TE-3-MD-HC: http://www.littlegiant.com/littlegiant/specsheet.nsf/SpecSheets/581604/$File/995779_TE-3-MDHC.pdf
Can somebody concur with what was suggested?.
many thanks
I have a 50 gallon tank containing a Black Oxide chemical solution for blackening metal.
Tank operating temp is 200 deg F.
the MSDS for this solution shows:
Sodium Hydroxide <30%
Sodium Nitrate <10%
Sodium Nitrate <1%
This concentrated basic solution gets mixed 50-50 with water.
I would...
Thank you very much gentlemen, I shall just keep the one I already have for a spare and get another made up out of one of the tool steels. I was thinking along the lines of a A7, seems to have a high wear resistance.
Thanks again.
I have a forming tool / press made from AISI 1144, and would like to know the best method to use to get the highest hardness / wear resistance. Strength and toughness do not matter for this application.
Should I even bother heat treating this part made from aisi 1144, or should we make...