PWHT is needed only once per weld over 38mm (CS, or 32mm if not preheated during welding).
If it has undergone PWHT already I would think only the new weld would be needing PWHT.
Same thing when making a vessel in two parts, pwht-ing them.
Then welding a closure seam and local pwht on the...