1.4404 resistant

Status
Not open for further replies.

Mechanical_weld

Mechanical
May 25, 2020
5
Hello,

what y thing about using stainless steel 1.4404 to about 2000ppm of chloride?
 
Replies continue below

Recommended for you

Stainless steel 1.4404 (equivalent to 316L) will not last long in a 2000 ppm chloride solution

This question has been asked and answered many times on eng-tips ...

MJCronin
Sr. Process Engineer
 
Thank you for your answer. So I'm gonna keep digging deeper in that case and go through that issue on eng-tips.
Also maybe you know what happen when the number of chloride solution increase above 2000?
 
Bad things, Nahmeeb .... bad things will happen ...

... and if by "digging deeper" you mean performing a single google search using the terms "eng-tips" "stainless" and "chlorides" in the search terms...

Yes, we really thing that you can do this !!!!.... Good luck on that, buddy !!!!

MJCronin
Sr. Process Engineer
 