1. Due to some incident on site some angles and beams were twisted around 20degrees.
Can these members retained on site retained to their original shape without effecting assumed elastic properties, procedure?advise?
 
Replies continue below

Recommended for you

Very doubtful.

Pictures?

At the very least these will be work hardened and properties impacted by the yielding.

Very unlikely to be worth the risk to retain them. They are now scrap metal.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Depends on the length of the angles and beams. The shorter the worse it will be.

If you can’t guarantee they weren’t yielded in a any way, scrap them.
 
I would say "no" to that as a general rule, but it depends on what exactly happened.

If they have been twisted to a new "permanent" geometry, that means that they have been accedentally "cold-formed". Then they will have built-in stresses due the partial plastic deformations.
Things like that can be analyzed to investigate the effect and at least get an idea regarding the residual stresses. But is it worth the effort?

Even if you manage to push them back to the original geometry, you will have a stress distribution that is affected by the yielding in the load history. It can perhaps be managed, but is it worth the effort [smile]?
 
My opinion is , fixing /straightening could be option if the profile low carbon mild steel and with flame straightenning process rather than cold bending or hammering..

I would remind also , fixing /straightening requires experienced workmanship..

If you write ( straightening steel beam ) and search the forum ,

some of the outcomes;

- thread507-106922

- thread607-377464...

The following video is useful to get flame straightening concept..






Tim was so learned that he could name a
horse in nine languages: so ignorant that he bought a cow to ride on.
(BENJAMIN FRANKLIN )
 
it is mild steel low carbon. if yielded not known. RFQ for heat process in process.
 
They yielded if they didn't bounce back to original shape.
 

Permanent deformation means material is yielded...If you continue to loading up to yield and unloading , the material will get strain hardening..


Hooke_s_Law_and_Modulus_of_Elasticity_oppagb.jpg






Tim was so learned that he could name a
horse in nine languages: so ignorant that he bought a cow to ride on.
(BENJAMIN FRANKLIN )
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor