We was rewound some synchronous 1KV wind generators and due to the high peak voltges the stator windings are failling.
The winding's analysis of the generator`s manufacturer reports that our job was good but ...........
1.The insulation thickness is not sufficient for Inverter fed winding.Overhang of phase insulation and is not sufficient for a inverter fed winding, it should be > 8 mm( 0.8 mm ?)
2.Leading out no protected with sleevings
3.The outlets from coils are not shrink wrapped to the winding end to provide more mechanicall fixture
4. The level for the varnish impegnation is not the standard quality for 1LA8 machines.
5. The Round wire with unknown insulation type, on surface there is probably diffusion barrier wich is not wettable/hydrophilic during the process of impregnation.
I would like to know if some one have a very good procedure including recommended materials to wind inverter proof this kind of wind generators.
Attached you will find the wire specs.
Thanks in advance fr the feed back and comments.
Regards
Petronila
We was rewound some synchronous 1KV wind generators and due to the high peak voltges the stator windings are failling.
The winding's analysis of the generator`s manufacturer reports that our job was good but ...........
1.The insulation thickness is not sufficient for Inverter fed winding.Overhang of phase insulation and is not sufficient for a inverter fed winding, it should be > 8 mm( 0.8 mm ?)
2.Leading out no protected with sleevings
3.The outlets from coils are not shrink wrapped to the winding end to provide more mechanicall fixture
4. The level for the varnish impegnation is not the standard quality for 1LA8 machines.
5. The Round wire with unknown insulation type, on surface there is probably diffusion barrier wich is not wettable/hydrophilic during the process of impregnation.
I would like to know if some one have a very good procedure including recommended materials to wind inverter proof this kind of wind generators.
Attached you will find the wire specs.
Thanks in advance fr the feed back and comments.