120" ID seamless SA516-70 pipe is available?

Oo.......
 
Replies continue below

Recommended for you

well 516-70 is a plate spec not a pipe spec

I think the largest pipe mill around is really 48" seamless

So, really, no.
 
Spiral weld pipe is probably available in that size. LB Foster (LBFOSTER.com) lists up to 96" on their web site. American Spiral Weld (ACIPCO.com)lists up to 144".
 
Since A-516 is plate, it can only be furnished in welded pipe. 120" diameter forgings are available which could be used to make seamless pipe.

 