Where can I find pressure-temperature ratings for 12 Chrome material (i.e., 410, 410S, 405, etc.)? B16.5 does not include 12Cr.
 
Replies continue below

Recommended for you

sb533023, correct, it does not, therefore you won't find them.

A common approach is to evaluate the design per a recognized Code, such as Sec VIII, Div 1, Apx 2 for flanges (and hope for the best).

Regards,

Mike
 