Veranium
Materials
- Aug 11, 2022
- 9
Does all 15-5 need to be cooled to 70F? We are wondering at my company if cooling 15-PH to 40F or below would give us better mechanical properties?
We usually get material that is with the .5-.7 range. My previous company used to require that we always held our manganese within the .75-.9 range. Is there any benefits in control the Mn or any of the alloying elements mainly Cr and Ni.
Thank you
We usually get material that is with the .5-.7 range. My previous company used to require that we always held our manganese within the .75-.9 range. Is there any benefits in control the Mn or any of the alloying elements mainly Cr and Ni.