Anybody knows which manufacturer makes the 16" Series "S" owsj?
i need the capacity.

Building location is Toronto, Canada.

Thanks
 
Replies continue below

Recommended for you

The "S" series was made back in the early 60's by a number of different manufacturers. Either contact SJI or purchase their catalog of old joists.

 
I show four 16" S-series joists. Which one did you need?
 
JD2,
can you share with me the specs for all 4 joists?

Thanks.
 
I show the last revision to the SJI for S series joists dated October 26, 1960 - the J series is indicated after this date. The first standard loading table showing the S series is dated June 26, 1958, effective January 1, 1959. Prior to this date I show the SJ series.

Web members are designed to a minimum of 50% max shear

16S5 Resisting moment 202,000 in lbs.
Approximate weight 7.5 plf
Maximum end reaction 3,000#
16S6 Resisting moment 242,000 in lbs.
Approximate weight 8.5 plf
Maximum end reaction 3,300#
16S7 Resisting moment 290,000 in lbs.
Approximate weight 10 plf
Maximum end reaction 3,600#
16S8 Resisting moment 336,000 in lbs.
Approximate weight 11.5 plf
Maximum end reaction 3,900#
 
Does anyone has the dimensions of the 16S5 joist?
 