Sep 5, 2014 #1 JPGraphX Mechanical Joined Oct 15, 2010 Messages 23 Location CA Hi! I would like to know if someone could help me find a North America equivalent for 16MnCr5. This is a material from germany. Thank you very much. JP
Hi! I would like to know if someone could help me find a North America equivalent for 16MnCr5. This is a material from germany. Thank you very much. JP
Sep 5, 2014 #2 EdStainless Materials Joined May 20, 2004 Messages 16,390 Location Waukesha WI USA Or 1.7131, It looks like a 5117 (UNS G51170) if I am reading my Stahlschlussel correctly. = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote
Or 1.7131, It looks like a 5117 (UNS G51170) if I am reading my Stahlschlussel correctly. = = = = = = = = = = = = = = = = = = = = Plymouth Tube
Sep 5, 2014 #3 CoryPad Materials Joined Apr 15, 2002 Messages 5,192 Location US There really isn't an equivalent because 16MnCr5 has higher Mn and Cr than 51XX steels. What product form do you need? 16MnCr5 is available in the USA in bar form, though the minimum quantities may not suit your application. Upvote 0 Downvote
There really isn't an equivalent because 16MnCr5 has higher Mn and Cr than 51XX steels. What product form do you need? 16MnCr5 is available in the USA in bar form, though the minimum quantities may not suit your application.
Sep 5, 2014 Thread starter #4 JPGraphX Mechanical Joined Oct 15, 2010 Messages 23 Location CA Well, 4 dowell pin hehehe.. Upvote 0 Downvote