I was wondering if anyone knows how high 17-4 material can be heated during solution without growing grain size. I know the recommended temp is 1900F but I'm wondering what will happen if the furnace is hotter(~1970F).
Thanks
 
Replies continue below

Recommended for you

Do you know what the original forging temperaure was? If it was higher than 1970 F, then grain growth should not be an issue.
 