Flesh
Materials
- Jul 17, 2003
- 108
I have specified round pins be made of 17-4 H1150 double-aged. I want to freeze these pins prior to insertion into bores. My first question, any metallurgical change that can occur during freezing step that should cause me concern?
Second question. My supplier, in their infinite wisdom, supplied me condition H1075 because it's "equal or better in strength and therefore meets my requirements". While I work with my purchasing team to unravel this debacle, same metallurgical question as above but for condition H1075.
Thank you for your time.
Second question. My supplier, in their infinite wisdom, supplied me condition H1075 because it's "equal or better in strength and therefore meets my requirements". While I work with my purchasing team to unravel this debacle, same metallurgical question as above but for condition H1075.
Thank you for your time.