I had disc-springs made of "equivalent" material to 17-7 PH called 1.4568 (european standard).
They are now completely broken and I don't know why. The machine has been out of use for two years near the sea... till they were going to use it.
The springs were loaded, but no vibration and no shocks at all.
Does anybody know if this material shows any type of "stress cracking" with H2S or marine environments?
ZZtop