Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations pierreick on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

1880 framing 5

Status
Not open for further replies.

ketco

Materials
Dec 3, 2023
1
Hello, looking for drawing details on 1800's framing.
Have 4 story building in need of repairs.
Large timber frame roof trusses support floors below (attic, 3rd, 2nd floors).
Tension rods extend from attic framing down to beams supporting the floor joists.
Before we perform selective demolition to inspect, would like to review any similar framing details.
Thank you.

 
Replies continue below

Recommended for you

Lumber sizes may be full size or larger, and careful for conditions of brown rot (aka dryrot).

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
ketco said:
Tension rods extend from attic framing down to beams supporting the floor joists.

Assume the rods are wrought iron, not steel. See this link for guidance on yield strength of historic wrought iron members.

 