I work at a machine shop that has got into fixing sawguides for certain customers, The guide consists of 1-1/2" aluminum, it is roughly 12" x 6". When a saw hits the guide it gauges the aluminum, which we either weld , or if its minimal we fill with devcon aluminum putty. We have been requested to apply a surface coating approxiamately 1mm thick to the guide after fixing to build up its thickness which is extremely critical. Does anyone know of a procedure or coating that can be applied to aluminum and in certain spots devcon that will build up the surface consistantly, and is rugged enough not to flake?
thanks.
welding would apply to much heat to one side and warp the guide, its also time consuming and expensive
 
Epoxy?

Why not mechanically attach (screws) a sacrifical plate (19ga) to the top of the guide. Replace as needed.

[green]"Art without engineering is dreaming; Engineering without art is calculating."[/green]
Steven K. Roberts, Technomad
Have you read faq731-376 to make the best use of Eng-Tips Forums?
 
Hard coat (not decorative anodize) puts up to .002" build of hard garnett surface on the aluminum. This is extremely durable and cannot be machined. I think it can be ground. It is extremely wear resistant.
 